Superiority:
Indium antimony (InSb) single crystal
1, process: the growth of indium antimonide single crystal by pull method;
2, purity: 6N(99.9999%);
3. Test: GDMS (the total of all impurity elements is less than 1ppm); XRD. Resistance test;
3, Specifications: Single crystal rod, wafer, wafer, thickness can be 0.3mm;
4, doping: tellurium or germanium;
5. Services: provide MSDS and practical protective measures; Provide material application solutions; Provide free samples;
Provide electron mobility, carrier concentration test report;
6, use: infrared detector parts, indium antimony magnetoresistance sensor;
Details:
Indium antimony (InSb) single crystal
1, process: the growth of indium antimonide single crystal by pull method;
2, purity: 6N(99.9999%);
3. Test: GDMS (the total of all impurity elements is less than 1ppm); XRD. Resistance test;
3, Specifications: Single crystal rod, wafer, wafer, thickness can be 0.3mm;
4, doping: tellurium or germanium;
5. Services: provide MSDS and practical protective measures; Provide material application solutions; Provide free samples;
Provide electron mobility, carrier concentration test report;
6, use: infrared detector parts, indium antimony magnetoresistance sensor;