NJ Colored Aliphati...

NJ Colored Aliphatic Polyurethane Topcoat

NJ Colored Aliphatic Polyurethane Topcoat

Min.Order / FOB Price:Get Latest Price

0 Metric Ton

Negotiable

  • Min.Order :0 Metric Ton
  • Purity: 40%-50%
  • Payment Terms : L/C,T/T

Keywords

NJ Colored Aliphatic Polyurethane Topcoat Aliphatic Polyurethane Topcoat Polyurethane Topcoat

Quick Details

  • Appearance:
  • Application:track vehicle automobile
  • PackAge:
  • ProductionCapacity:|Metric Ton|Day
  • Storage:
  • Transportation:

Superiority:

The film is excellent in decorative,bright,plump and high gloss; excellent mechanical properties,toughness, abrasion resistance,weatherability,excellent color protection, no powdering, yellowing resistance; excellent water resistance and chemical resistance.
 

Details:

Product Introduction
It’s composed of specific hydroxy acrylic resin,pigment, solvent, additives as paint part,and isocyanate as curing agent part.
Product Features
The film is excellent in decorative,bright,plump and high gloss; excellent mechanical properties,toughness, abrasion resistance,weatherability,excellent color protection, no powdering, yellowing resistance; excellent water resistance and chemical resistance.
Recommended Use
High grade agricultural machinery or accessories
Typical Application Of Coating
Colored electrophoretic primer + NJ colored aliphatic polyurethane topcoat
NJ colored acrylic polyurethane finish + NJ colored aliphatic polyurethane topcoat
NJ colored epoxy primer + NJ colored aliphatic polyurethane topcoat
Construction Method
Air spray
Use Note
Put the curing agent into the paint according to the ratio before painting, and the qty should be according to the requirements, use it within 4hours after mixing.
Keep the tools dry and clean;
Keep the surface clean, no moisture, no acid and alkali;
Keep the painting process far away from water, acid, alkali, alcohol and other contact.
Curing agent is easy to react with water, alcohol and other things, the hardener drum must be covered in order to avoid damaged by damp cementation;

The working humidity shall not be greater than 80%, otherwise it will cause serious film foam

 

Related cases

Case Diagram Of Agricultural Machinery Industry

Related Searches

Confirm to collect the product to my collection?

OKCancel

About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia

Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog

©2008 LookChem.com,License: ICP

NO.:Zhejiang16009103

complaints:service@lookchem.com Desktop View