Rubber homogenizing...

Rubber homogenizing agents 40MS

Rubber homogenizing agents 40MS

Min.Order / FOB Price:Get Latest Price

1 Kilogram

Negotiable

  • Min.Order :1 Kilogram
  • Purity: 100%
  • Payment Terms : L/C,D/A,D/P,T/T,

Keywords

Rubber homogenizing agents Rubber tackifying agent struktol 40MS 40MSF 60NS

Quick Details

  • Appearance:dark brown nonhardening resin compound
  • Application:Rubber homogenizing agentRubber tackifying agent
  • PackAge:20kgs/bag or as customers' request
  • ProductionCapacity:30,000|Metric Ton|Year
  • Storage:well-ventilation cool, dry area
  • Transportation:not dangerous goods

Superiority:

Rubber homogenizing agents 40MS

capacity:30,000mts/year

stable quality 

competitive price 

accept PSI such as SGS,BV,CIQ

ISO9001  14001

Details:

<p>  </p> <p> <strong>Rubber homogenizing agents 40MS</strong></p> <p> <strong>(Struktol 40MS, 40MSF,60NSF equivalent)</strong></p> <div> tackifying agent</div> <p> AU-40MS;AU-40MSF;AU-60NSF</p> <p>  </p> <p> <strong>Specification:</strong></p> <table> <tbody> <tr> <td> <p> <img src="file:///C:\DOCUME~1\ADMINI~1\LOCALS~1\Temp\ksohtml\wps_clip_image-10668.png" /></p> </td> <td> <p> Appearance</p> </td> <td> <p> Softening point,℃</p> </td> <td> <p> Ash %</p> </td> <td> <p> Remarks</p> </td> </tr> <tr> <td> <p> AU-40MS</p> </td> <td> <p> dark brown nonhardening resin </p> <p> compound</p> </td> <td> <p> 50~60</p> </td> <td> <p> ≤0.5</p> </td> <td> <p> 40MS</p> </td> </tr> <tr> <td> <p> AU-40MSF</p> </td> <td> <p> Dark brown pastilles</p> </td> <td> <p> 96~106</p> </td> <td> <p> ≤2</p> </td> <td> <p> 40MSF</p> </td> </tr> <tr> <td> <p> AU-60NS</p> </td> <td> <p> Amber-colored pastilles</p> </td> <td> <p> 95~105</p> </td> <td> <p> ≤2</p> </td> <td> <p> 60NSF</p> </td> </tr> </tbody> </table> <p>  </p> <p> <strong>Application and characteristics: </strong></p> <p> This can promote the products of different polarity rubber mixing, and to improve its compatibility, improved technology performance, to close Lian, a refining and rolling operations. To integrate more closely compound, thus enhancing coal mixed results, distributed better, more evenly mixed, enhancing compound uniformity. Apart from increasing compound viscous, but also to improve their mobility, enhance the mechanical properties of the finished vulcanization.<br /> In butyl rubber-based formula, in addition to improving the processing performance, promote fill scattered, aging can still maintain a low modulus of good viscous and upgrade compound extrusion performance, improve tolerance flexor flexible, but also enhance compound Hermetic. In addition to improving the synthetic rubber molding viscous; of carbon black and mineral filler has an excellent role in the decentralized, low-temperature impact of buckling.</p> <p> <strong>Package and storage:</strong><br /> 20kgs/bag or as customer’s request;</p> <p> Stock in well-ventilation cool, dry area. </p> <p>  </p> <p> <strong>contact:</strong></p> <p> linda zhu:  0086-13625427538</p> <p> skype yahoo: alliswellcome</p>

Related Searches

Confirm to collect the product to my collection?

OKCancel

About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia

Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog

©2008 LookChem.com,License: ICP

NO.:Zhejiang16009103

complaints:service@lookchem.com Desktop View