    Thin films of tungsten selenides (WSex) were obtained by using a method of shadow-masked pulsed laser deposition. The deposition at room temperature of substrates caused the formation of Se-enriched amorphous films (Se/W∼5) with pronounced surface roughness because of an effective nanoparticle growth. Heating or DC biasing the substrate during the deposition modified the film composition (Se/W∼1.7 – 4) and resulted in the smoothing of the film surface. Annealing the films, deposited at room temperature, as well as heating the substrate during the deposition caused crystallization of the films. Catalytic activity of WSex thin films in hydrogen evolution reaction (HER) was studied in 0.5 M H2SO4 aqueous solution at room temperature. The structural state and the chemical composition of WSex films had an expressed impact on the catalytic activity. A significant improvement in HER activity was observed in the case of Se-enriched films deposition followed by annealing at 500 °C.

    We also recommend Trading Suppliers and Manufacturers of TUNGSTEN SELENIDE (cas 12067-46-8). Pls Click Website Link as below: cas 12067-46-8 suppliers


    Prev:Synthesis and thermoelectric performance of titanium diboride and its composites with lead selenide and carbon
    Next: Synthesis process and thermoelectric properties of n-type tin selenide thin films)

About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia

Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog

©2008 LookChem.com,License: ICP

NO.:Zhejiang16009103

complaints:service@lookchem.com Desktop View