Boron carbide (cas 12069-32-8) submicron powder was synthesized with boron oxide and graphene as starting materials by gas-solid reaction method using two different apparatuses. The effects of calcination temperature and holding time, apparatus type and B2O3/C ratio of the starting materials on the phase composition and morphology of the synthesized powders were evaluated. A newly formed residual carbon morphology distinct from original graphene were present in samples synthesized at a higher B2O3/C ratio or temperature. The synthesis temperature of ∼1500 °C was found to be more suitable to obtain boron carbide powder without the existence of residual carbon. The new type of apparatus enabled the synthesis of boron carbide phase at a relatively lower temperature, due to its more efficient use of B2O3 vapor.
We also recommend Trading Suppliers and Manufacturers of Boron carbide (cas 12069-32-8). Pls Click Website Link as below: cas 12069-32-8 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View