To reduce the negative effects of lizardite on the flotation of pentlandite, amino trimethylene phosphonic acid(ATMP) was tested as a potential depressant for lizardite. Micro-flotation test results indicated that the flotability of pentlandite restored in pentlandite-lizardite system by the addition of ATMP. The adsorption and ICP results indicated that ATMP interacted with the Mg species of lizardite surface meanwhile a part of the Mg ions were dissolved from lizardite surface. XPS tests illustrated that ATMP changed the surface characteristics of lizardite mineral and the Mg/Si atomic ratio decreased on lizardite surface. Zeta potential measurements demonstrated that the lizardite zeta potential was changed from positive to negative after interacting with ATMP, which caused the electro-steric repulsion between pentlandite and lizardite particles, and thus the pentlandite floatability was restored.
We also recommend Trading Suppliers and Manufacturers of lizardite (cas 12161-84-1). Pls Click Website Link as below: cas 12161-84-1 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View