Lanthanum-doped titanium-zirconium-molybdenum (La-TZM) alloy was prepared by powder metallurgy and rolling process. The processing crack and crack initiation mechanisms of La-TZM alloy after sintering, hot rolling and cold rolling were studied by scanning and transmission electron microscopy. The results show that the doped La(NO3)3, TiH2 and ZrH2 have finer secondary phase in the La-TZM alloy plate. The fracture mode of sintering billet is inter-granular, but the fracture surface of hot rolling exhibited transgranular cleavage. However, the cold rolling is quasi-cleavage fracture. The secondary phase particles tend to hinder the movement of dislocations causing dislocations pile-up. The resulting tensile stress can accelerate cracks nucleation and growth, and the crack propagation will be deflected by the secondary phase particles. The crack initiation can be avoided by reducing local stress concentration caused by dislocations.
We also recommend Trading Suppliers and Manufacturers of lanthanum titanium trioxide (cas 12201-04-6). Pls Click Website Link as below: cas 12201-04-6 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View