Add time:08/05/2019 Source:sciencedirect.com
Spark Plasma Sintering has been used to obtain first ever fine-grained SrWO4 and NaNd(WO4)2 ceramics with the scheelite structure and high density (95.8–99%) that are promising as materials for nuclear waste immobilization. It has been demonstrated that the densification intensity in tungstates at the initial sintering stage is determined by the agglomeration degree of input powders. The activation energy of fine-grained ceramics with the scheelite structure has been established to correlate at high temperatures with the activation energy of grain-boundary diffusion. Rapid sintering of fine-grained NaNd(WO4)2 ceramic results in internal tensile stress fields that lead to lowered hardness and fracture toughness of the ceramic.
We also recommend Trading Suppliers and Manufacturers of STRONTIUM TUNGSTATE (cas 13451-05-3). Pls Click Website Link as below: cas 13451-05-3 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View