The preparation of ZnO nanoparticles with a multi-step process is reported. The preparation path included zinc hydroxide nitrate (ZnHN) or zinc hydroxide carbonate (ZnHC) precipitation, their thermal treatment and nano-milling. ZnO preparation was followed in detail by STEM, FT-IR, XRD and TG-MS analyses. In order to demonstrate the efficiency of the nano-milling process, the obtained ZnO nanoparticles were characterized with regard to their photo-catalytic activity of caffeine degradation. The smallest ZnO nanoparticles (∼20 nm) with the highest BET surface (∼80 m2 g−1) were prepared from ZnHC at 300 °C.
We also recommend Trading Suppliers and Manufacturers of Zinc carbonate hydroxide (cas 12539-71-8). Pls Click Website Link as below: cas 12539-71-8 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View