Strength of a soldered palladium alloy, PGC (Engelhard Corp.), and a soldered medium gold alloy, PGX (Engelhard Corp.), was examined. The results obtained were as follows:1. Highest strength was observed with postsoldered specimens of PGC alloy.2. Microstructural examination of postsoldered specimens revealed nearly pore-free solder joints with PGC and PGX alloys, and fracture appeared at the solder-alloy interface with PGC and PGX alloys.3. Microstructural examination of presoldered and presoldered/thermocycled specimens revealed that presoldered specimens of PGC and PGX alloys exhibited intrasolder fracture; PGX solder joints had considerably less porosity, which may explain the equivalent bond strengths of all the soldered specimens and the yield point of the controls; PGC solder joints exhibited large quantities of pores, which may explain the lower strength; pores observed in PGC alloy may be the result of the high fusing temperature of the solder; and these results indicate a need to develop a new presolder for PGC.4. The best result was obtained with postsoldered specimens of the PGC alloy. However, for PGX alloy, either postsolder or presolder techniques can be used.
We also recommend Trading Suppliers and Manufacturers of palladium alloy PGC (cas 107373-32-0). Pls Click Website Link as below: cas 107373-32-0 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View