Add time:07/17/2019 Source:sciencedirect.com
Monophase Calcium zirconate (cas 12013-47-7) (CaZrO3) has been prepared from the equimolar ZrO2 + CaCO3 mixture by two-step synthesis process. In the first step, mechanical treatment of the mixture is performed in an AGO-2 planetary ball mill. In the second step, the milled mixture is annealed to form calcium zirconate. High-energy ball milling of the (ZrO2+CaCO3) mixture results in decrease in the temperature of CaZrO3 formation during annealing at 950 °C. The enhancement of CaZrO3 synthesis is due to accumulation of excess energy by the reagents, decreasing the particle size and notable increase in the interphase area because of “smearing” of CaCO3 on ZrO2 particles during milling. Nanocrystalline calcium zirconate has been produced by controlling the annealing temperature and time.
We also recommend Trading Suppliers and Manufacturers of Calcium zirconate (cas 12013-47-7). Pls Click Website Link as below: cas 12013-47-7 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View