    The efficiency of silicon removal technology by acid leaching and flocculation during zirconium oxychloride octahydrate (ZrOCl2⋅8 H2O) production has been improved. The optimum conditions of acid leaching were found to be as follows: transiton material, 300 g; HCl (6 mol/L), 600 mL; leaching time, 4 h; and leaching temperature, 100 °C. The nonionic polyoxyethylene lauryl ether (AEO9) was adopted as the flocculant. The optimum flocculation conditions were found to be as follows: temperature, 40 °C; flocculant amount, 10 ml (concentration 1%); time, 1 h. The zirconium oxychloride solution after purification contained 36 ppm SiO2 and 160 g/L ZrOCl2. The polymerization and flocculation mechanisms of silicic acid were analyzed. Results of Fourier-transform infrared, scanning electron microscopy, nuclear magnetic resonance, and Brunauer–Emmett–Teller analyses showed the main transformation and properties of the products in the acid leaching and flocculation processes.

    We also recommend Trading Suppliers and Manufacturers of Silicic acid, sodium zirconium salt (cas 12738-56-6). Pls Click Website Link as below: cas 12738-56-6 suppliers


    Prev:Short Communicationγ-ORYZANOL (cas 12738-23-7) ameliorates the acute stress induced by behavioral anxiety testing in mice
    Next: ArticleThree-dimensional model for stellacyanin (cas 12738-61-3), a “blue” copper-protein☆)

About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia

Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog

©2008 LookChem.com,License: ICP

NO.:Zhejiang16009103

complaints:service@lookchem.com Desktop View