  • Thermo-oxidative ageing behavior of CERIUM OXIDE (cas 1345-13-7)/silicone rubber☆
  • Add time:08/31/2019         Source:sciencedirect.com

    Cerium oxide/silicon rubber was prepared via mechanical blending. Mechanical and frictional properties, as well as thermal stability after thermo-oxidative ageing were investigated in this rubber composite. 3D surface profilometry, scanning electron microscopy (SEM) and thermogravimetry analysis (TGA) were used to study the friction surface characteristics, friction mechanism and thermal stability, respectively. Additionally, swelling experiments were carried out to investigate the variation of crosslinking density. After thermo-oxidative ageing, the tear strength of cerium oxide/silicon rubber decreases. However, in the early ageing stage, improvements in tensile strength, elongation at break, and frictional performance are caused by crosslinking density increments. Moreover, the addition of cerium oxide remarkably improves the re-crosslinking degree during ageing process, which in turn decreases the number of holes on the friction surface and endows the silicon rubber with better mechanical and frictional properties, as well as thermo-oxidative ageing resistance.

    We also recommend Trading Suppliers and Manufacturers of CERIUM OXIDE (cas 1345-13-7). Pls Click Website Link as below: cas 1345-13-7 suppliers


    Prev:Survey of mercury, cadmium and lead content of household batteries☆
    Next: Full Length ArticleExperimental study on evaporation characteristics of diesel/CERIUM OXIDE (cas 1345-13-7) nanofluid fuel droplets)

About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia

Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog

©2008 LookChem.com,License: ICP

NO.:Zhejiang16009103

complaints:service@lookchem.com Desktop View