Add time:09/09/2019 Source:sciencedirect.com
TaNx thin films were grown at temperatures ranging from 200 to 375 °C using atomic layer deposition (ALD). PENTAKIS(DIMETHYLAMINO)TANTALUM (cas 19824-59-0) (PDMAT) was used as a tantalum source with either ammonia or monomethylhydrazine (MMH) as a nitrogen co-reactant. Self-limiting behaviour was observed for both ammonia and MMH processes, with growth rates of 0.6 and 0.4 Å/cycle, respectively at 300 °C. Films deposited using ammonia were found to have a mono-nitride stoichiometry with resistivities as low as 70 mΩ cm. In contrast, films deposited using MMH were found to be nitrogen rich Ta3N5 with high resistivities. A Quartz Crystal Microbalance (QCM) was used to measure mass gain and loss during the cyclic ALD processes and the data was used in combination with medium energy ion scattering (MEIS) to elucidate the PDMAT absorption mechanisms.
We also recommend Trading Suppliers and Manufacturers of PENTAKIS(DIMETHYLAMINO)TANTALUM (cas 19824-59-0). Pls Click Website Link as below: cas 19824-59-0 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View