The NiCoCrAlY alloy with uniform yttrium distribution was fabricated via powder milling and spark plasma sintering. After powder milling, yttrium was uniformly distributed in the alloy in the form of Ni-Y precipitates (50–150 nm) and nano-sized Y2O3 particles (5–30 nm). It was found that the uniform yttrium distribution could: 1) lower thermally grown oxides (TGO) growth rate; 2) reduce the growth stress in the TGO; 3) suppress S segregation to the interface and the formation of interfacial imperfections (e.g. oxide intrusions, pores). Consequently, the oxidation and spallation resistance of the TGO was significantly improved.
We also recommend Trading Suppliers and Manufacturers of Yttrium oxide (cas 1314-36-9). Pls Click Website Link as below: cas 1314-36-9 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View