Add time:07/21/2019 Source:sciencedirect.com
Erbium-doped SiO2-TiO2 thin films were prepared by the sol-gel method, using erbium nitrate pentahydrate powder, tetraethyl-orthosilicate (TEOS), and titanium tetraisopropoxide (TTIP) as precursors. The Si/Ti ratios in the SiO2-TiO2 films agree with the TEOS/TTIP molar ratio in the sol-gel precursor. Atomic coordination structure of erbium was defined by extended X-ray absorption fine structure spectrometry (EXAFS) and optical properties of the films were characterized by micro-photoluminescence (Micro-PL). The first-neighbor-shell coordination number of erbium in SiO2-TiO2 thin films would influence the optical properties. The 700 °C-annealed 80%SiO2-20%TiO2:Er1.0% (mol%) film with the lowest coordination number exhibits the highest photoluminescence intensity. Moreover, Fourier transform infrared spectroscopy (FTIR) analysis reveals that the main bonding structures of SiO2-TiO2 thin films are related to the erbium dopants. The modification of microstructure and chemical bonding configuration in the SiO2-TiO2 films by the Er-doping concentration and its influence on the optical properties are discussed.
We also recommend Trading Suppliers and Manufacturers of Erbium(III) nitrate (cas 10168-80-6). Pls Click Website Link as below: cas 10168-80-6 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View