    The low-temperature calcination of nickel sulphide concentrates with sodium chloride and subsequent hydrometallurgical processing is a promising alternative methods. This study aims to identify the interaction products of sulphide nickel concentrate components with sodium chloride at temperatures of 400–450 °C. Thermodynamic studies have demonstrated that nickel sulphates, chlorides, and oxides are the probable nickel-containing products of the interaction between nickel sulphide and sodium chloride in the presence of oxygen. At 350–450 °C, the formation of nickel sulphate is preferred; as the temperature increases, the probability of oxide formation also increases. We experimentally confirmed that nickel sulphate is the main nickel-containing product of the reaction between nickel sulphide concentrate and sodium chloride at 400 °C, and the reduced nickel oxide and chloride content was identified in the calcine. The other main products included iron oxide (III) and sodium sulphate. During calcination at 400 °C, up to 75% of the sulphur contained in the concentrate was bound to sodium sulphate.

    We also recommend Trading Suppliers and Manufacturers of NICKEL SULFIDE (cas 11113-75-0). Pls Click Website Link as below: cas 11113-75-0 suppliers


    Prev:NICKEL SULFIDE (cas 11113-75-0) cathode for stable charge-discharge rates in lithium rechargeable battery
    Next: Solution combustion synthesis of NICKEL SULFIDE (cas 11113-75-0) composite powders)

About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia

Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog

©2008 LookChem.com,License: ICP

NO.:Zhejiang16009103

complaints:service@lookchem.com Desktop View