The aim of this study was to produce dense, single phase polycrystals. The research was carried out on the submicron tungsten carbide powder without additives, with either a carbon or tungsten additive and on the powder with both additives. The primary task of carbon was to reduce surface oxide impurities which passivate WC grains; tungsten in turn bounds free carbon in the WC. The authors manufactured fine-grained, dense (96–98% T.D.) and single-phase WC polycrystals, using the technique of pressureless sintering at the temperature not exceeding 2000 °C. A positive effect of carbon addition on tungsten carbide sinterability was observed, whereby a dense, fine-grained polycrystals can be obtained at 1900 °C. It was also observed that a significant excess of temperature of sintering process resulted in a strong abnormal grain growth of WC grains.
We also recommend Trading Suppliers and Manufacturers of Tungsten carbide (cas 11130-73-7). Pls Click Website Link as below: cas 11130-73-7 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View