carbon black rubber tire
This product is suitable for all kinds of natural rubber and synthetic rubber, easily dispersed, which can give rubber high resistance, high extrusion speed, smooth extrusion surface, small orifice expansion. Vulcanized rubber is high temperature resistance and good thermal conductivity, reinforcement, better flexibility and resilience. Mainly used in tire cord layer, sidewall, and extrusion, rolled products, rubber compound. This product is best for the butyl rubber inner tube and used with the N660.
|
SPECIFICATION | TEST DATA | TEST METHOD | ||||||||||
Iodine Absorption Number g/kg | 43±5 | 43 | GB/T 3780.1 | ||||||||||
Nitrogen surface area 10m³㎡/kg | 35-45 | 39 | GB/T 10722 | ||||||||||
STSA 103m2/kg | 34-44 | 38 | GB/T 10722 | ||||||||||
CTAB Absorption Area 103m2/kg | 36-48 | 42 | GB/T 3780.5 | ||||||||||
Oil Absorption Number(Method A) 105m3/kg | 121±7 | 120 | GB/T 3780.2 | ||||||||||
Compressed Oil Absorption Number 10-5m3/kg | 80-90 | 85 | GB/T 3780.4 | ||||||||||
Ash Content % | ≤0.7 | 0.25 | GB/T 3780.10 | ||||||||||
Residue on 45um Sieve mg/kg | ≤1000 | 200 | GB/T 3780.21 | ||||||||||
Impurity | NO | NO | GB/T 3780.12 | ||||||||||
Loss on Heating % | ≤1.5 | 0.5 | GB/T 3780.8 | ||||||||||
Tint Strength % | *** | *** | *** | ||||||||||
Pour Density kg/m3 | 360±40 | 335 | GB/T 14853.1 | ||||||||||
|
-0.5±1.5 | -0.8 | GB/T 3780.18 |
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View