Rubber antioxidant 4010NA/IPPD

Rubber antioxidant 4010NA/IPPD

Min.Order / FOB Price:Get Latest Price

1 Metric Ton

FOB Price: USD 2450.0000

  • Min.Order :1 Metric Ton
  • Purity: 96%
  • Payment Terms : L/C,D/P,T/T

Keywords

CAS NO:101-72-4 Rubber additive 4010NA/IPPD N-isopropyl-N’-phenyl-p-phenylene diamine

Quick Details

  • Appearance:Dark brown to dark violet pastilles
  • Application:Mainly used in manufacture of tires , rubber shoes and other rubber products .
  • PackAge:25KG/BAG
  • ProductionCapacity:150|Metric Ton|Day
  • Storage:in cool place
  • Transportation:Aavoid exposing to sun.

Superiority:

                 RubberAntioxidant4010NA(IPPD)   

 

Item

Quality Grade

Appearance

Dark brown to dark violet pastilles .

Melting Point

70.0℃ MIN

Heating loss

0.30% MAX

Ash

0.20% MAX

Assay(GC)

95.0% MIN

 

Details:

Rubber Antioxidant IPPD(4010NA)

Commodity Name :Rubber Antioxidant 4010NA(IPPD)

Chemical Name : N-isopropyl-N’-phenyl-p-phenylene diamine

Chemical Structure:

Molecular Formula: C15H18N2

Molecular Weight: 226.31

CAS NO.:101-72-4

Quality standard : GB/T 8828-2003

Specification:

 

 

Item

Quality Grade

Appearance

Dark brown to dark violet pastilles .

Melting Point

70.0℃ MIN

Heating loss

0.30% MAX

Ash

0.20% MAX

Assay(GC)

95.0% MIN

 

 

 

 

 

 

 

 

 

 

 

Properties: A high activity antioxidant fmatural synthetic rubber provides powerful antiozonant antioxidant properties with excellent high temperature, fatigue flex resistance to rubber compounds. While used primarily fozone resistance, it is a more active antioxidant than quinoline diphenylamine based antioxidants. The product (alone in combination with TMQ) provides compound protection against catalytic degradation by copper other heavy metals. The product has no negative effects on compound adhesion to textiles steel cord up to levels of 2 phr. Above this concentration it may bloom interfere with ply to ply ply to cord adhesion. It will discolcompounds cause severe contact migration staining.

 

Application: Used in pneumatic tire components, solid tires, belts, hoses, cables, automotive mounts, bushings general mechanical products that are exposed to continuous intermittent dynamic operating conditions require protection from ozonation.

 

Packing : 25kg plastic woven bag, paper with plastic film bag, kraft paper bag.

 

Storage: Store closed containers in a cool, dry, well-ventilated area, store far from strong oxidizing materials. Avoid exposure to direct sunlight. Do not double stack

Related Searches

Confirm to collect the product to my collection?

OKCancel

About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia

Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog

©2008 LookChem.com,License: ICP

NO.:Zhejiang16009103

complaints:service@lookchem.com Desktop View