Add time:08/02/2019 Source:sciencedirect.com
Experiments are conducted in the W-Si system to understand the diffusion mechanism of the species. The activation energies from integrated diffusion coefficients are calculated as 152 ± 7 and 301 ± 40 kJ/mol in the WSi2 and W5Si3 phases, respectively. In both the phases, Si has a much higher diffusion rate compared to W. This is not surprising to find in the WSi2 phase, if we consider the number of nearest neighbors for both the elements in the crystal. The diffusion of W in this phase indicates the presence of W antisites. The faster diffusion rate of Si in the W5Si3 phase indicates the presence of higher concentration of vacancies on the Si sublattice compared to W sublattice.
We also recommend Trading Suppliers and Manufacturers of TUNGSTEN SILICIDE (cas 12039-88-2). Pls Click Website Link as below: cas 12039-88-2 suppliers
About|Contact|Cas|Product Name|Molecular|Country|Encyclopedia
Message|New Cas|MSDS|Service|Advertisement|CAS DataBase|Article Data|Manufacturers | Chemical Catalog
©2008 LookChem.com,License: ICP
NO.:Zhejiang16009103
complaints:service@lookchem.com Desktop View