Dielectric permittivity has been measured for some ternary mixtures of poly(ε-caprolactone), poly(4-chlorostyrene) and dioxane at 25°C. The relaxation time due to the longitudinal component of the ester-group dipole in the polylactone chain increases roughly linearly with increasing total polymer concentration at a rate in rough agreement with earlier dielectric data for binary systems.